He aha nā kumu o nā hemahema kuʻihao maʻamau i ka hui PCB?

Ma ke kaʻina hana oNā papa kaapuni hui PCB, ʻaʻole hiki ke ʻike ʻia nā hemahema wili a me nā hemahema ke ʻano.ʻO kēia mau mea e hoʻopilikia iki i ka papa kaapuni.I kēia lā, hoʻopuka kēia ʻatikala i nā kikoʻī i nā hemahema wili maʻamau, nā hiʻohiʻona hiʻohiʻona, nā pōʻino a me nā kumu o ka PCBA.E nānā kākou E nānā iā ia!

Pseudo Soldering

Nā hiʻohiʻona hiʻohiʻona:aia ka palena ʻeleʻele maopopo ma waena o ka mea kūʻai aku a me ke keʻokeʻo o nā ʻāpana a i ʻole ke keleawe keleawe, a ua pohō ka mea kūʻai aku i ka palena.

Pilikia:hiki ʻole ke hana maʻamau.

ʻIkepili kumu:

1. ʻAʻole hoʻomaʻemaʻe ʻia nā alakaʻi ʻāpana, uhi ʻia a i ʻole oxidized.

2. ʻAʻole i hoʻomaʻemaʻe maikaʻi ʻia ka papa i paʻi ʻia, a ʻaʻole maikaʻi ka maikaʻi o ka flux sprayed.

ʻO ka hōʻiliʻili solder

Nā hiʻohiʻona hiʻohiʻona:ʻO ke ʻano o ka hui solder he ʻoluʻolu, keʻokeʻo a ʻeleʻele. 

Ka Ike Kumu:

1. ʻAʻole maikaʻi ka maikaʻi solder.

2.ʻAʻole lawa ka mahana soldering.

3. I ka wā i hoʻopaʻa ʻole ʻia ai ka solder, wehe nā alakaʻi ʻāpana.

 hui pcb

Nui loa ka solder

Nā hiʻohiʻona hiʻohiʻona:He convex ka ʻili solder.

Nā pōʻino:Hoʻopili ʻia nā ʻōpala a loaʻa paha nā hemahema.

ʻIkepili kumu:Ua lohi loa ka hoʻokuʻu ʻana i ka solder.

 

Liʻiliʻi solder

Nā hiʻohiʻona hiʻohiʻona:ʻOi aku ka liʻiliʻi o ka wīwī ma lalo o 80% o ka pad, a ʻaʻole i hana ka solder i kahi hoʻololi maʻalahi.

Pilikia:ʻAʻole lawa ka ikaika mechanical.

Ka Ike Kumu:

1.Poor solder kahe a i'ole ka ha'alele mua 'ana o ka solder.

2. Insufficient flux.

3.Welding manawa pōkole loa.

 

Kuʻi ʻo Rosin

Nā hiʻohiʻona hiʻohiʻona:Loaʻa ka ʻōpala rosin i ka weld.

Nā pōʻino:ʻAʻole lawa ka ikaika, maikaʻi ʻole ka hoʻokele ʻana, a hiki ke hele a i waho.

Ka Ike Kumu:

1. He nui nā mīkini wiliwili a i ʻole i hāʻule.

2.ʻAʻole lawa ka manawa wili a lawaʻole ka hoʻomehana.

3.ʻAʻole weheʻia ke kiʻi oxide ma kaʻili.

 

Ka wela nui

Nā hiʻohiʻona hiʻohiʻona:nā hui kuʻi keʻokeʻo, ʻaʻohe ʻulaʻula metala, ʻili ʻeleʻele.

Pilikia:He maʻalahi ka ʻili a hoʻemi ʻia ka ikaika.

ʻIkepili kumu:

Nui loa ka mana o ka hao hao a lōʻihi ka manawa hoʻomehana.

 

Kuʻi anu

Nā hiʻohiʻona hiʻohiʻona:ʻO ka ʻili he mau ʻāpana e like me ka bean curd, a i kekahi manawa he māwae paha.

Pilikia:ikaika haʻahaʻa, haʻahaʻa uila conductivity.

ʻIkepili kumu:Aia ka jitter ma mua o ka paʻa ʻana o ka solder.

 

Hoʻokomo maikaʻi ʻole

Nā hiʻohiʻona hiʻohiʻona:ʻO ka pilina ma waena o ka solder a me ka weldment he nui loa a ʻaʻole maʻalahi.

Pilikia:ka haʻahaʻa haʻahaʻa, ʻaʻohe pili a i ʻole pili ʻana.

Ka Ike Kumu:

1. ʻAʻole maʻemaʻe ka weldment.

2. ʻAʻole lawa a maikaʻi ʻole ka maikaʻi.

3.ʻAʻole i wela pono nā Weldments.

 

Asymmetrical

Nā hiʻohiʻona hiʻohiʻona:ʻAʻole kahe ka solder i ka pad.

Pilikia:ʻAʻole lawa ka ikaika.

Ka Ike Kumu:

ʻAʻole maikaʻi ʻo 1.Solder fluidity.

2. ʻAʻole lawa a maikaʻi ʻole ka maikaʻi.

3.ʻAʻole lawa ka wela.

 

wehe

Nā hiʻohiʻona hiʻohiʻona:Hiki ke hoʻoneʻe ʻia nā uea a i ʻole nā ​​mea alakaʻi.

Pilikia:ʻilihune a ʻaʻohe alakaʻi.

Ka Ike Kumu:

1. Ke neʻe nei ke alakaʻi ma mua o ka paʻa ʻana o ka solder, e hoʻoheheʻe ʻia.

2. ʻAʻole mākaukau maikaʻi nā alakaʻi (ʻilihune a ʻaʻole i pulu).

 

ʻOi ʻana

Nā hiʻohiʻona hiʻohiʻona:ʻO ke ʻano o kahi piko.

Pilikia:maikaʻi ʻole ke ʻano, maʻalahi ke kumu o ka hoʻopili ʻana.

Ka Ike Kumu:

1. ʻAʻole liʻiliʻi ka flux a lōʻihi loa ka manawa hoʻomehana.

2. ʻAʻole kūpono ke kihi o ka hao hao e hoʻihoʻi.

Hui PCB

Hoʻopili ʻana

Nā hiʻohiʻona hiʻohiʻona:Hoʻopili ʻia nā uea pili.

Pilikia:Kaapuni pōkole uila.

Ka Ike Kumu:

1. Nui loa solder.

2. ʻAʻole kūpono ke kihi o ka hao hao e hoʻihoʻi.

  

ʻāʻī

Nā hiʻohiʻona hiʻohiʻona:Aia nā puka i ʻike ʻia e ka nānā ʻana a i ʻole ka hoʻonui haʻahaʻa.

Pilikia:ʻAʻole lawa ka ikaika, maʻalahi nā ami solder e ʻino.

ʻIkepili kumu:Nui loa ka ʻokoʻa ma waena o ke poʻo a me ka lua pad.

 

 

ʻōhū

Nā hiʻohiʻona hiʻohiʻona:ʻO ke kumu o ke kēpau he puʻupuʻu puhi ahi, a he lua i loko.

Pilikia:ʻO ka conduction manawa, akā he maʻalahi ke kumu o ka hana maikaʻi ʻole no ka manawa lōʻihi.

Ka Ike Kumu:

1. ʻO ke āpau ma waena o ke alakaʻi a me ka lua pad he nui.

2.Poor pulu kepau.

3. Ua lōʻihi ka manawa kuʻi o ka papa ʻaoʻao ʻelua ma o nā lua, a hoʻonui ka ea i loko o nā lua.

 

ʻO ka makaihoʻokiʻekiʻe ʻia i kēlā me kēia pahu

Nā hiʻohiʻona hiʻohiʻona:Hoʻopili ʻia ka pahu keleawe mai ka papa i paʻi ʻia.

Pilikia:Ua poino ka papa i paiia.

ʻIkepili kumu:He lōʻihi loa ka manawa wiliwili a kiʻekiʻe loa ka mahana.

 

Peel

Nā hiʻohiʻona hiʻohiʻona:Hoʻopili ʻia nā hui solder mai ka pahu keleawe (ʻaʻole ka pahu keleawe a me ka papa i paʻi ʻia).

Pilikia:Kaapuni hamama.

ʻIkepili kumu:ʻAʻole i hoʻopaʻa ʻia ka metala ma ka pā.

 

Ma hope o ka nānā 'ana i nā kumu oHoʻohui ʻia ʻo PCBnā hemahema, hilinaʻi mākou i ka hāʻawi ʻana iā ʻoe i ka hui maikaʻi loahuli-ki PCB lawelawe hui, ka maikaʻi, ke kumu kūʻai a me ka manawa hāʻawi i kāu ʻāpana liʻiliʻi liʻiliʻi PCB hui kauoha a me ka Mid batch Volume PCB kauoha hui.

Inā ʻoe e ʻimi nei i kahi mea hana hui PCB kūpono, e ʻoluʻolu e hoʻouna i kāu faila BOM a me nā faila PCB i sales@pcbfuture.com.He hūnā loa kāu mau faila a pau.E hoʻouna mākou iā ʻoe i kahi ʻōlelo pololei me ka manawa alakaʻi i nā hola 48.

 